It is described the production of crystalline 2,3 disyndiotactic polynorbornene with a decomposition (without melting) temperature in the range 380-400 °C characterized by insolubility in aromatic hydrocarbons at room temperature and partially soluble in boiling toluene. The production procedure, the crystal structure and new clathrate structures of PNB formed by polymeric helices with tubular internal cavities are also described.
NORBORNENE POLYMERS AND COPOLYMERS WITH A STEREOREGULAR 2,3 DISYNDIOTACTIC STRUCTURE: PREPARATION PROCESSES AND CLATHRATE STRUCTURES INVOLVING THE SAID MACROMOLECULES
FAMULARI, ANTONINO;MEILLE, STEFANO VALDO;
2010-01-01
Abstract
It is described the production of crystalline 2,3 disyndiotactic polynorbornene with a decomposition (without melting) temperature in the range 380-400 °C characterized by insolubility in aromatic hydrocarbons at room temperature and partially soluble in boiling toluene. The production procedure, the crystal structure and new clathrate structures of PNB formed by polymeric helices with tubular internal cavities are also described.File in questo prodotto:
File | Dimensione | Formato | |
---|---|---|---|
PMI01301-WO-Pubblicazione A1.pdf
Accesso riservato
:
Altro materiale allegato
Dimensione
947.24 kB
Formato
Adobe PDF
|
947.24 kB | Adobe PDF | Visualizza/Apri |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.