The nucleation of apatite and calcium phosphates onto natural polysaccharides containing carboxyl groups can be obtained by immersion in biomimetic solutions. The deposition of hydroxyapatite has been recently described also on pectin, and pectin–apatite hybrid gels were proposed as scaffolds for bone tissue regeneration. In this work, injectable calcium phosphate/pectin microspheres were prepared to promote both the natural process of biomineralization and the controlled release of encapsulated cells, genes, enzymes, proteins or drugs in the pathological situ. Pectin microspheres were prepared with different formulations from aqueous solutions using an extrusion system, and incubated in H2O or SBF for 14 days. The presence of an excess of CaCl2, deriving from the preparation process, was determinant in promoting the deposition of calcium phosphates from SBF, whereas no mineral deposition was detected on pectin microspheres extensively purified after preparation. The nucleation of calcium phosphates occurred on pectin microspheres incubated in SBF for 14 days and was evaluated through ESEM–EDS analysis and FT-IR spectroscopy.

Mineral phase deposition on pectin microspheres

MUNARIN, FABIOLA;GIULIANO, LILIANA;BOZZINI, SABRINA;TANZI, MARIA CRISTINA;PETRINI, PAOLA
2010-01-01

Abstract

The nucleation of apatite and calcium phosphates onto natural polysaccharides containing carboxyl groups can be obtained by immersion in biomimetic solutions. The deposition of hydroxyapatite has been recently described also on pectin, and pectin–apatite hybrid gels were proposed as scaffolds for bone tissue regeneration. In this work, injectable calcium phosphate/pectin microspheres were prepared to promote both the natural process of biomineralization and the controlled release of encapsulated cells, genes, enzymes, proteins or drugs in the pathological situ. Pectin microspheres were prepared with different formulations from aqueous solutions using an extrusion system, and incubated in H2O or SBF for 14 days. The presence of an excess of CaCl2, deriving from the preparation process, was determinant in promoting the deposition of calcium phosphates from SBF, whereas no mineral deposition was detected on pectin microspheres extensively purified after preparation. The nucleation of calcium phosphates occurred on pectin microspheres incubated in SBF for 14 days and was evaluated through ESEM–EDS analysis and FT-IR spectroscopy.
2010
Pectin; microspheres; SBF; biomineralization; bone regeneration
File in questo prodotto:
File Dimensione Formato  
Mineral phase deposition on pectin microspheres.pdf

Accesso riservato

: Post-Print (DRAFT o Author’s Accepted Manuscript-AAM)
Dimensione 766.48 kB
Formato Adobe PDF
766.48 kB Adobe PDF   Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11311/570037
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 28
  • ???jsp.display-item.citation.isi??? 20
social impact