Inconel 625 is a nickel alloy designed for environments characterized by severe stress and corrosive conditions, such as aerospace, marine, and petrochemical fields. Since nickel alloys have no transformation temperatures, grain refinement is only achievable through recrystallization. Nevertheless, during the solution treatment or when high temperature deformation is inadequate, grain coarsening can occur with a consequent decrease of the mechanical characteristics. In these cases, an aging treatment can be helpful to recover partially or completely the tensile properties. Even though Alloy 625 is generally not included among the age-hardening alloys, the new API STANDARD 6ACRA allows the aging treatment after solution treatment. The formation of γ’’ precipitates at temperatures included between 570°C and 750°C can increase the mechanical resistance significantly. However, over 700°C the formation of Cr-rich carbides is highly detrimental for the corrosion properties. This work investigates the influence of the aging treatment on the tensile and the corrosion characteristics varying the grain size. The impact of precipitation hardening is essential when mechanical strength is compromised by a coarse grain structure. Since the phases formed during the heat treatment can impair the corrosion resistance, experimental tests are necessary to collect both mechanical and corrosion resistance data.
Influence of aging treatment and grain size on the mechanical and corrosion properties of Alloy 625
R. Gerosa;B. Rivolta;M. Tenca;
2026-01-01
Abstract
Inconel 625 is a nickel alloy designed for environments characterized by severe stress and corrosive conditions, such as aerospace, marine, and petrochemical fields. Since nickel alloys have no transformation temperatures, grain refinement is only achievable through recrystallization. Nevertheless, during the solution treatment or when high temperature deformation is inadequate, grain coarsening can occur with a consequent decrease of the mechanical characteristics. In these cases, an aging treatment can be helpful to recover partially or completely the tensile properties. Even though Alloy 625 is generally not included among the age-hardening alloys, the new API STANDARD 6ACRA allows the aging treatment after solution treatment. The formation of γ’’ precipitates at temperatures included between 570°C and 750°C can increase the mechanical resistance significantly. However, over 700°C the formation of Cr-rich carbides is highly detrimental for the corrosion properties. This work investigates the influence of the aging treatment on the tensile and the corrosion characteristics varying the grain size. The impact of precipitation hardening is essential when mechanical strength is compromised by a coarse grain structure. Since the phases formed during the heat treatment can impair the corrosion resistance, experimental tests are necessary to collect both mechanical and corrosion resistance data.| File | Dimensione | Formato | |
|---|---|---|---|
|
26_048.pdf
Accesso riservato
:
Publisher’s version
Dimensione
709.63 kB
Formato
Adobe PDF
|
709.63 kB | Adobe PDF | Visualizza/Apri |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.