Hard–soft interfaces (HSIs) enable mechanically dissimilar materials to be combined but are susceptible to strain localization and preferential fracture. Inspired by natural graded interfaces, we investigate voxel-based functionally graded materials (FGMs) to enhance HSI fracture and progressive damage resistance. Co-continuous hard-to-soft transitions with different gradient coefficients were fabricated by multi-material 3D printing and characterized under quasi-static and incremental cyclic loading. Among the investigated configurations, α = 0.5 provided the most favorable strength–energy absorption balance. Relative to the non-graded Control, it increased fracture stress by 10.2 %, energy density to fracture by 30.0 %, and total energy density to failure by 22.6 % under quasi-static loading. Under incremental cyclic loading, it exhibited a 14.5 % higher total cyclic energy–density response, 3.0 % higher fracture stress, and 2.9 % more cycles sustained before failure. Digital image correlation and crack-path observations revealed broader strain redistribution, crack deflection into the compliant phase, and delayed crack coalescence. These results show that grading primarily modifies progressive damage and fracture pathways and that HSI performance depends on both constituent phase fractions and their spatial distribution, establishing voxel-scale grading as a strategy for designing damage-tolerant multi-material structures.

Enhancing fracture and cyclic damage resistance of hard-soft interfaces via voxel-based functionally graded materials

Buccino, F.;Vergani, L. M.;
2026-01-01

Abstract

Hard–soft interfaces (HSIs) enable mechanically dissimilar materials to be combined but are susceptible to strain localization and preferential fracture. Inspired by natural graded interfaces, we investigate voxel-based functionally graded materials (FGMs) to enhance HSI fracture and progressive damage resistance. Co-continuous hard-to-soft transitions with different gradient coefficients were fabricated by multi-material 3D printing and characterized under quasi-static and incremental cyclic loading. Among the investigated configurations, α = 0.5 provided the most favorable strength–energy absorption balance. Relative to the non-graded Control, it increased fracture stress by 10.2 %, energy density to fracture by 30.0 %, and total energy density to failure by 22.6 % under quasi-static loading. Under incremental cyclic loading, it exhibited a 14.5 % higher total cyclic energy–density response, 3.0 % higher fracture stress, and 2.9 % more cycles sustained before failure. Digital image correlation and crack-path observations revealed broader strain redistribution, crack deflection into the compliant phase, and delayed crack coalescence. These results show that grading primarily modifies progressive damage and fracture pathways and that HSI performance depends on both constituent phase fractions and their spatial distribution, establishing voxel-scale grading as a strategy for designing damage-tolerant multi-material structures.
2026
Functionally graded materials, Hard-soft interfaces, Voxel-based design, Multi-material additive manufacturing, Fracture resistance, Cyclic damage resistance
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S0264127526020897-main_compressed.pdf

accesso aperto

: Publisher’s version
Dimensione 2.47 MB
Formato Adobe PDF
2.47 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11311/1333434
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
  • OpenAlex 0
social impact