Structures may collapse during the cooling phase of a fire, yet standard furnace tests only measure the response under heating. There lacks experimental test protocols and design methods to assess resistance until burnout. This paper describes a new experimental approach for burnout resistance evaluation, reports experimental data on loaded reinforced concrete columns in furnace tests with cooling down phases, and presents numerical models of the tests. The test results show that columns designed for a standard fire resistance of 60 min exhibited a fire resistance of 83 min in the furnace but failed during the cooling phase when the burners were shut off after 72 min while the load was maintained. Two other specimens survived exposure to heating of 45 and 55 min, respectively, and their residual capacity was measured. Finite element analyses show agreement with the tests, showing applicability of numerical methods for evaluating burnout resistance of concrete columns. These findings demonstrate experimentally that delayed thermal-mechanical effects can jeopardize structural stability in real fires, and provide a framework to measure these effects. Moving beyond fire resistance to quantify the response until burnout will support designs for safety of occupants and firefighters throughout the fire and promote repairability and resilience.

Experimental investigation of structural failure during the cooling phase of a fire: concrete columns

Felicetti R.;Bamonte P.;
2022-01-01

Abstract

Structures may collapse during the cooling phase of a fire, yet standard furnace tests only measure the response under heating. There lacks experimental test protocols and design methods to assess resistance until burnout. This paper describes a new experimental approach for burnout resistance evaluation, reports experimental data on loaded reinforced concrete columns in furnace tests with cooling down phases, and presents numerical models of the tests. The test results show that columns designed for a standard fire resistance of 60 min exhibited a fire resistance of 83 min in the furnace but failed during the cooling phase when the burners were shut off after 72 min while the load was maintained. Two other specimens survived exposure to heating of 45 and 55 min, respectively, and their residual capacity was measured. Finite element analyses show agreement with the tests, showing applicability of numerical methods for evaluating burnout resistance of concrete columns. These findings demonstrate experimentally that delayed thermal-mechanical effects can jeopardize structural stability in real fires, and provide a framework to measure these effects. Moving beyond fire resistance to quantify the response until burnout will support designs for safety of occupants and firefighters throughout the fire and promote repairability and resilience.
2022
Fire tests
Concrete columns
Structural failure
Cooling phase
Burnout resistance
Numerical model
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S0379711222001680-main.pdf

Accesso riservato

Descrizione: Articolo completo
: Post-Print (DRAFT o Author’s Accepted Manuscript-AAM)
Dimensione 5.15 MB
Formato Adobe PDF
5.15 MB Adobe PDF   Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11311/1234855
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 7
  • ???jsp.display-item.citation.isi??? 3
social impact